| Category | Polymer , Adhesive , Thermoset , Silicone |
| Manufacturer | Dow Corning |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Dow Corning SE 1896 FR KIT.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.980 - 0.990 g/cc @Temperature 25.0 °C |
0.980 - 0.990 g/cc @Temperature 77.0 °F |
|
| Viscosity | 380 cP | 380 cP | dynamic |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Penetration P(0), 1/10 mm | 53 | 53 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 150 °C | 302 °F | |
| Minimum Service Temperature, Air | -45.0 °C | -49.0 °F |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Dielectric Constant | 3.1 @Frequency 1.00e+6 Hz |
3.1 @Frequency 1.00e+6 Hz |
|
| Dielectric Strength | 20.0 kV/mm | 508 kV/in |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 60.0 min @Temperature 70.0 °C |
1.00 hour @Temperature 158 °F |
|
| Shelf Life | 15.0 Month | 15.0 Month |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | translucent | |
| Flowable | yes | |
| Gel Hardness (Grams/Penetration) | 105 | |
| Hydrophobic | yes | |
| Self Leveling | yes | |
| Water Resistant | yes | |
| Working Time (min) | >240 |