Dow Corning 431 HS RESIN

Category Polymer , Thermoset , Silicone
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 431 HS RESIN.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
High solids version of Dow Corning® 840 resin. Medium hardness resin for maintenance paints, colored baking enamels and decorative finishes. Improves heat resistance and weathering of organic resins.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc

@Temperature 25.0 °C
1.14 g/cc

@Temperature 77.0 °F
Volatile Organic Compounds (VOC) Content 228 g/l
228 g/l
Volatiles 20 %
20 %
Thermal Properties Metric English Comments
Flash Point 7.00 °C
44.6 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 33.0 Month
33.0 Month
Descriptive Properties Value Comments
Water Resistant yes