Meehanite K-325 Austempered Ductile Iron

Category Metal , Ferrous Metal , Cast Iron , Alloy Cast Iron , Ductile Iron
Manufacturer Meehanite
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Meehanite K-325 Austempered Ductile Iron.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type K-325 is used for applications such as gears requiring high contact rolling and tooth bending fatigue properties. Type K-325 also possess high fracture toughness impact strength. Excellent founding properties enable more accurate castings with savings in machine stock required. Damping capacity and notch sensitivity are superior to steel castings and forgings. Self-lubricating properties make Type K-405 ideal for wear conditions involving minimal lubrication.General Meehanite information - Meehanite metal is first melted to a definite degree of undercooling or constitution which is related to the section of the casting to be poured and the range of physical properties such as tensile strength and hardness required. Nucleation with patented mixtures of graphitizing agents results in the removal of undercooling, in the controlled precipitation of graphite and in a fine grained eutectic cell structure which determines the density and physical integrity of the casting. Ordinary cast irons made to chemical specifications which do not include the benefit of controlled undercooling are influenced by mass effect to a maximum degree and for this and other reasons cannot be considered an equivalent to Meehanite metal.Information provided by Meehanite Marketing Association.
Mechanical Properties Metric English Comments
Hardness, Brinell 300 - 350
300 - 350
Tensile Strength, Ultimate 1000 MPa
145000 psi
Tensile Strength, Yield 772 MPa
112000 psi
Elongation at Break 5.0 - 8.0 %
5.0 - 8.0 %
Fatigue Strength 324 MPa
47000 psi
Endurance Limit (Notched)
455 MPa
66000 psi
Endurance Limit (Unnotched)