Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

DSM Novamid® 1015G50 NA/BK37 PA6-GF50

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 50% Glass Fiber Filled
Manufacturer DSM Engineering Plastics
Trade Name Novamid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Novamid® 1015G50 NA/BK37 PA6-GF50.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
50% Glass Reinforced, Injection Molding
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
dry; ISO 1183
Moisture Absorption 1.70 %
1.70 %
Sim. To ISO 62
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 230 MPa
33400 psi
dry; ISO 527-1/-2
Elongation at Break 4.1 %
4.1 %
dry; ISO 527-1/-2
Tensile Modulus 15.0 GPa
2180 ksi
dry; ISO 527-1/-2
Flexural Strength 370 MPa
53700 psi
dry; ISO 178
Flexural Modulus 1.60 GPa
232 ksi
dry; ISO 178
Charpy Impact Unnotched 10.5 J/cm²

@Temperature 23.0 °C
50.0 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²

@Temperature 23.0 °C
9.52 ft-lb/in²

@Temperature 73.4 °F
dry; ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3