DSM Fibre Intermediates Nyrim® 3000 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer DSM Fibre Intermediates
Trade Name Nyrim®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF DSM Fibre Intermediates Nyrim® 3000 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) technology. Nyrim® is a registered trademark.Information provided by the manufacturer, Brueggemann Chemical.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ISO 868
Tensile Strength, Ultimate 37.0 MPa
5370 psi
ISO 527
Elongation at Break 350 %
350 %
ISO 527
Modulus of Elasticity 0.978 GPa
142 ksi
ISO 527
Flexural Modulus 1.045 GPa
151.6 ksi
ISO 178
Shear Modulus 0.450 GPa
65.3 ksi
torsional
Izod Impact, Notched (ISO) 62.0 kJ/m²
29.5 ft-lb/in²
ISO 180, Ductile break
16.0 kJ/m²

@Temperature -40.0 °C
7.61 ft-lb/in²

@Temperature -40.0 °F
Ductile break; ISO 180
Charpy Impact, Notched 4.20 J/cm²
20.0 ft-lb/in²
DIN 53453, Ductile break
2.80 J/cm²

@Temperature -40.0 °C
13.3 ft-lb/in²

@Temperature -40.0 °F
Ductile break; DIN 53453
Thermal Properties Metric English Comments
Melting Point 213 °C
415 °F
DSC