Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179 |
Iran Petrochemical (PCC) BL6 HM7255 High Density Polyethylene BL6 (HM 755) is a high density polyethylene with Butene-1 as a comonomer. It is a high molar mass material with very good impact strength, stiffness, and stress cracking resistance.Applications: la.. |
|||
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® ST25G7 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eU |
Lucite International Diakon® TD642 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | ISO 179/1eA |
Borealis Daplen™ EE040AE TPO Compound Daplen EE040AE is an elastomer modified polypropylene compound intended for injection molding. Daplen EE040AE is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansi.. |
|||
Charpy Impact, Notched | 4.20 J/cm² @Temperature 23.0 °C |
20.0 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
CP-Polymer-Technik Wellamid® 6000/58 GV 15 HWUVCP 15% Glass Fiber Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | DIN 53453, Ductile break |
DSM Fibre Intermediates Nyrim® 1500 (Conditioned) Conditioned at 23°C and 50% Relative Humidity.Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is proc.. |
|||
Charpy Impact, Notched | 4.20 J/cm² | 20.0 ft-lb/in² | DIN 53453, Ductile break |
DSM Fibre Intermediates Nyrim® 3000 (Dry) Nyrim is a Block Copolymer of Nylon 6 and an elastomer with exceptional properties in impact resistance, fatigue and abrasion resistance. Nyrim is processed via Reaction Injection Moulding (RIM) tec.. |