Material Notes:
Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt viscosities to suit all extrusion processes: barrier and coating film, tube and hose, monofilament, stock shapes. Akulon resins are characterized by:consistent qualityhigh purity for film applications, low gel contents. Molding ResinsSuited to all engineering demands: Unfilled low and medium viscosity gradesToughened unfilled gradesGlass reinforced from 20-45% filledLow warpage reinforced gradesFlame retardant; UL V0 rated and glow wire typesHalogen free FR gradesBlow moldable materialsLaser markable resinsLaser weldable, high burst pressure gradesToughened, reinforced resinsHigh stiffness grades for metal replacement Akulon Ultraflow resins have high flow with mechanical properties similar to standard materials. Exceptional flow allows: productivity gains in moldinglower built in stressesbetter surface appearancesystem cost reductions Applications for Molding resins There is an Akulon resin available suitable for any application requiring polyamides. Key areas where DSM has specific application knowledge areAutomotiveUnder the hood and engine componentsExterior and interior applicationsElectrical components and connectorsElectricalLow voltage power distributionLightingPower connectorsConsumer DurablesPower and lawn and garden toolsSmall AppliancesSports and leisure equipmentFurniture accessoriesIndustrial GoodsTransportation (railways)Information provided by DSM.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Water Absorption 7.6 %
7.6 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 2.3 %
2.3 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 130 MPa
18900 psi
ISO 527-1/-2
Elongation at Break 3.5 %
3.5 %
ISO 527-1/-2
Tensile Modulus 6.00 GPa
870 ksi
ISO 527-1/-2
Charpy Impact Unnotched 4.50 J/cm²
<br>@Temperature -30.0 °C
21.4 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eU
5.00 J/cm²
<br>@Temperature 23.0 °C
23.8 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.700 J/cm²
<br>@Temperature -30.0 °C
3.33 ft-lb/in²
<br>@Temperature -22.0 °F
ISO 179/1eA
0.800 J/cm²
<br>@Temperature 23.0 °C
3.81 ft-lb/in²
<br>@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
<br>@Temperature 20.0 °C
16.7 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
<br>@Temperature 20.0 °C
44.4 µin/in-°F
<br>@Temperature 68.0 °F
ISO 11359-1/-2
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
UL RTI, Electrical 150 °C
<br>@Thickness 1.50 mm
302 °F
<br>@Thickness 0.0591 in
UL746B
150 °C
<br>@Thickness 0.710 mm
302 °F
<br>@Thickness 0.0280 in
UL746B
UL RTI, Mechanical with Impact 120 °C
<br>@Thickness 0.710 mm
248 °F
<br>@Thickness 0.0280 in
UL746B
125 °C
<br>@Thickness 1.50 mm
257 °F
<br>@Thickness 0.0591 in
UL746B
UL RTI, Mechanical without Impact 150 °C
<br>@Thickness 0.710 mm
302 °F
<br>@Thickness 0.0280 in
UL746B
150 °C
<br>@Thickness 1.50 mm
302 °F
<br>@Thickness 0.0591 in
UL746B
Flammability, UL94 HB
<br>@Thickness 1.60 mm
HB
<br>@Thickness 0.0630 in
IEC 60695-11-10
HB
<br>@Thickness 0.710 mm
HB
<br>@Thickness 0.0280 in
IEC 60695-11-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
IEC 60093
Dielectric Constant 3.5
<br>@Frequency 100 Hz
3.5
<br>@Frequency 100 Hz
IEC 60250
4.7
<br>@Frequency 1e+6 Hz
4.7
<br>@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 25.0 kV/mm
635 kV/in
IEC 60243-1
Dissipation Factor 0.0055
<br>@Frequency 100 Hz
0.0055
<br>@Frequency 100 Hz
IEC 60250
0.018
<br>@Frequency 1e+6 Hz
0.018
<br>@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 425 V
425 V
IEC 60112
400 - 599 V
400 - 599 V
PLC 1; UL 746A
Descriptive Properties Value Comments
Heat stabilized or stable to heat Yes
Injection molding Yes
Release Agent Yes
With Fillers Yes