Material Notes:
The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier film, stock shapes, convoluted tubes, and monofilament. Akulon XP is a high-productivity, high-performance PA6 grade for film extrusion processes. Medium viscosity, unreinforced or reinforced Akulon grades are used for various injection molding and blow molding applications. Akulon® Ultraflow® is a high-productivity, high-performance PA6 family for molding processes.Key applications for Akulon: Automotive: Intake manifold, Engine, Powertrain, Airbag containers, Exterior trim, Interior trim, Electrical components and connectorsConsumer durables: Power tools, Lawn and garden tools, Small appliances, Sports and leisure equipment, Furniture, Industrial Goods, TransportationE&E: Low voltage switch gear/power distribution, Lighting, Power connectorsFilm: Specialty and barrier filmsInformation provided by DSM.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Water Absorption 8.0 %
8.0 %
Sim. to ISO 62
Moisture Absorption at Equilibrium 2.4 %
2.4 %
Humidity Absorption; Sim. to ISO 62
Mechanical Properties Metric English Comments
Tensile Strength at Break 135 MPa
19600 psi
ISO 527-1/-2
Elongation at Break 4.0 %
4.0 %
ISO 527-1/-2
Tensile Modulus 7.20 GPa
1040 ksi
ISO 527-1/-2
Charpy Impact Unnotched 8.00 J/cm²

@Temperature 23.0 °C
38.1 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 1.10 J/cm²

@Temperature 23.0 °C
5.24 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 215 °C
419 °F
ISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 195 °C
383 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Blow Molding Yes
Heat stabilized or stable to heat Yes
With Fillers Yes