Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® Hardener

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Cytec
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.Cytec (Conap) FR-1272 Conapoxy® Resin / Conacure® HardenerLow cost, low viscosity, low exotherm potting and casting system.Mix Ratio, Resin/Hardener (by weight): 100/7 Cure Type: Room Temperature
Physical Properties Metric English Comments
Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 6.00e+14 ohm-cm
<= 6.00e+14 ohm-cm
Dielectric Constant 4.8

@Frequency 1000 Hz
4.8

@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Dissipation Factor 0.014

@Frequency 1000 Hz
0.014

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 180 - 300 min

@Temperature 60.0 °C
3.00 - 5.00 hour

@Temperature 140 °F
1440 - 2880 min

@Temperature 25.0 °C
24.0 - 48.0 hour

@Temperature 77.0 °F
Pot Life 90.0 min

@Temperature 25.0 °C
90.0 min

@Temperature 77.0 °F
100 grams