Cytec (Conap) FR-1047 / EA-117 Conapoxy® Resin / Conacure® Hardener

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Cytec
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec (Conap) FR-1047 / EA-117 Conapoxy® Resin / Conacure® Hardener.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive and related industries.Cytec (Conap) FR-1047 / EA-117 Conapoxy® Resin / Conacure® HardenerFlame retardant (UL 94V-0), filled, non-abrasive casting system with excellent thermal shock resistance, low exotherm, very good arc resistance, and high heat distortion properties.Mix Ratio, Resin/Hardener (by weight): 100/7 Cure Type: Elevated Temperature
Physical Properties Metric English Comments
Viscosity 26000 cP

@Temperature 25.0 °C
26000 cP

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 155 °C
311 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 2.00e+15 ohm-cm
<= 2.00e+15 ohm-cm
Dielectric Constant 5.4

@Frequency 1000 Hz
5.4

@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in
Dissipation Factor 0.026

@Frequency 1000 Hz
0.026

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 150 °C
2.00 hour

@Temperature 302 °F
Pot Life 480 min

@Temperature 25.0 °C
480 min

@Temperature 77.0 °F