Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Henkel Hysol EA 9695 Film Adhesive

Category Polymer , Adhesive , Film , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol EA 9695 Film Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Second generation, low flow, composite bonding film; excellent environmental resistance. Composite structure repair, cure and co-cure with composite laminates. Qualified to Airbus. Data from .050 psf, 250 g / m2.Applications: Composite Bonding Metal and Honeycomb Bonding Composite Surfacing
Physical Properties Metric English Comments
Storage Temperature -18.0 °C
-0.400 °F
Mechanical Properties Metric English Comments
Tensile Strength 8.30 MPa
1200 psi
Flatwise
Adhesive Bond Strength 19.3 MPa

@Temperature 132 °C
2800 psi

@Temperature 270 °F
Composite double overlap shear
30.3 MPa

@Temperature -55.0 °C
4390 psi

@Temperature -67.0 °F
Composite double overlap shear
34.5 MPa

@Temperature 25.0 °C
5000 psi

@Temperature 77.0 °F
Composite double overlap shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air >= 149 °C
>= 300 °F
Glass Transition Temp, Tg 86.0 °C
187 °F
wet, 121°C cure
95.0 °C
203 °F
wet, 175°C cure
122 °C
252 °F
dry, 121°C cure
150 °C
302 °F
dry, 175°C cure
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 177 °C
1.50 hour

@Temperature 351 °F
90.0 min

@Temperature 121 °C
1.50 hour

@Temperature 250 °F
Descriptive Properties Value Comments
Out-Time (days) 90
at 25°C