Material Notes:
CPM Rex 45 is an 8% cobalt modification of M3 high speed steel made by the CPM (Crucible Particle Metallurgy) Process. It has red hardness comparable to that of M42 but offers abrasion resistance even better than that of M3. With its excellent red hardness, good wear resistance and good toughness, CPM Rex 45 is suitable for difficult machining applications or high cutting speed applications.The CPM process results in a homogeneous microstructure with a finer, more uniform carbide distribution imparting superior dimensional stability, grindability and toughness when compared to steels produced by conventional processes. The CPM process also allows the design of more highly alloyed grades which cannot be produced by conventional steelmaking.Information provided by Crucible Specialty Metals.
Physical Properties Metric English Comments
Density 8.05 g/cc
0.291 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 255 - 285
255 - 285
Annealed
Hardness, Rockwell C 65
65
Hardening Temperature- 1165°C; Tempering Temperature- 560°C
67
67
Hardening Temperature- 1190°C; Tempering Temperature- 550°C
Modulus of Elasticity 214 GPa
31000 ksi
Flexural Strength 4709 MPa
683000 psi
Hardening Temperature- 1165°C, Tempering Temperature- 560°C
4826 MPa
700000 psi
Hardening Temperature- 1190°C, Tempering Temperature- 550°C
Charpy Impact 20.0 J
14.8 ft-lb
Hardening Temperature- 1190°C; Tempering Temperature- 550°C
27.0 J
19.9 ft-lb
Hardening Temperature- 1165°C; Tempering Temperature- 560°C
Thermal Properties Metric English Comments
CTE, linear 11.5 µm/m-°C

@Temperature 20.0 - 595 °C
6.39 µin/in-°F

@Temperature 68.0 - 1100 °F
Component Elements Properties Metric English Comments
Carbon, C 1.3 %
1.3 %
Chromium, Cr 4.05 %
4.05 %
Cobalt, Co 8.0 %
8.0 %
Iron, Fe 72.13 %
72.13 %
As Remainder
Molybdenum, Mo 5.0 %
5.0 %
Sulfur, S 0.060 - 0.22 %
0.060 - 0.22 %
Tungsten, W 6.25 %
6.25 %
Vanadium, V 3.05 %
3.05 %
Descriptive Properties Value Comments
Grindability; Metal Removed/Wheel Worn 4