Momentive Performance Materials TUFELâ„¢ II 94306 Low Volatile Extrusion Heat Cured Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Momentive Performance Materials (Former GE Silicones)
Trade Name TUFEL™ II
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Momentive Performance Materials TUFELâ„¢ II 94306 Low Volatile Extrusion Heat Cured Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance standards.TUFEL II Low Volatile 94306 is a member of the Addition Curing Portfolio. It is a platinum (addition/heat) curable, one-part compound. This product has been optimized for extrusion and calendering processes and is intended for application in the Healthcare industry.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 28
28
Tensile Strength 9.30 MPa
1350 psi
Elongation at Break 1050 %
1050 %
Tear Strength 30.0 kN/m
171 pli
Die B
Optical Properties Metric English Comments
Transmission, Visible 20 %
20 %
translucent; thickness unknown
Compliance Properties Metric English Comments
FDA Yes
Yes
FDA Indirect food contact - Rubber articles intended for repeated use - FDA Reg 21CFR177.2600
USP Class VI Yes
Yes
USP Class VI methods: Intramuscular implantation, intracutaneous injection, & systematic injection
Descriptive Properties Value Comments
Appearance Translucent
BfR product is compositionally compliant
Recommendation XV Silicones; post cured (4h/200°C)