Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Covestro Texin® 985U Urethane Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer Covestro
Trade Name Texin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® 985U Urethane Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingFilm extrusionProfile extrusionSheet extrusionBlow moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.12 g/cc
0.0405 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Yield 5.00 MPa

@Strain 50.0 %
725 psi

@Strain 50.0 %
Elongation at Break >= 50 %
>= 50 %
Thermal Properties Metric English Comments
Vicat Softening Point 80.0 °C
176 °F
50°C/h 50N
Glass Transition Temp, Tg -46.0 °C
-50.8 °F
10°C/min
Processing Properties Metric English Comments
Melt Temperature 195 °C
383 °F
Injection Molding
Mold Temperature 35.0 °C
95.0 °F
Injection Molding
Injection Pressure 45.0 MPa
6530 psi