Material Notes:
Desmopan 192 is a TPU on the basis of a standard ester.Applications: Castors, coupling elements, seals.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore A 94
94
DIN 53505
Hardness, Shore D 42
42
DIN 53505
Elongation at Break >= 50 %
>= 50 %
Nominal
Compression Set 25 %
25 %
70 hr; 22°C
60 %

@Temperature 70.0 °C
60 %

@Temperature 158 °F
24 hr
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 224 µm/m-°C

@Temperature 20.0 °C
124 µin/in-°F

@Temperature 68.0 °F
Electrical Properties Metric English Comments
Electrical Resistivity 5.00e+12 ohm-cm
5.00e+12 ohm-cm
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
Dielectric Constant 5.1

@Frequency 1e+6 Hz
5.1

@Frequency 1e+6 Hz
6.6

@Frequency 100 Hz
6.6

@Frequency 100 Hz
Dielectric Strength 14.8 kV/mm
376 kV/in
Dissipation Factor 0.025

@Frequency 100 Hz
0.025

@Frequency 100 Hz
0.075

@Frequency 1e+6 Hz
0.075

@Frequency 1e+6 Hz