Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer Covestro
Trade Name Bayflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Bayflex® XGT-80 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0085 cm/cm
0.0085 in/in
Bayer Test
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 26.0 MPa
3770 psi
ASTM D638/D412
Elongation at Break 150 %
150 %
ASTM D638/D412
Flexural Modulus 0.580 GPa
84.1 ksi
ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
Tear Strength 110 kN/m
628 pli
Die C; ASTM D624
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 20.0 °C
61.1 µin/in-°F

@Temperature 68.0 °F
ASTM D696