| Category | Polymer , Thermoplastic , ABS Polymer , Polycarbonate/ABS Alloy, Unreinforced , Polycarbonate (PC) |
| Manufacturer | Covestro |
| Trade Name | Bayblend® |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Covestro Bayblend® FR3001 PC/ABS Blend.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.18 g/cc | 0.0426 lb/in³ | ISO 1183-1 |
| Moisture Absorption at Equilibrium | 0.20 % | 0.20 % | ISO 62, 50% RH |
| Water Absorption at Saturation | 0.50 % | 0.50 % | ISO 62 |
| Viscosity | 150000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 260 °C |
150000 cP <br>@Shear Rate 1000 1/s,<br> Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
| Linear Mold Shrinkage, Flow | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.00 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
| Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm <br>@Thickness 3.00 mm |
0.0050 - 0.0070 in/in <br>@Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 50.0 MPa | 7250 psi | 50 mm/min; ISO 527-1,-2 |
| Tensile Strength, Yield | 60.0 MPa | 8700 psi | 50 mm/min; ISO 527-1,-2 |
| Elongation at Break | >= 30 % | >= 30 % | 50 mm/min; b.o. ISO 527-1,-2 |
| Elongation at Yield | 4.0 % | 4.0 % | 50 mm/min; ISO 527-1,-2 |
| Tensile Modulus | 2.70 GPa | 392 ksi | 1 mm/min; ISO 527-1,-2 |
| Izod Impact, Notched (ISO) | 8.00 kJ/m² <br>@Temperature -30.0 °C |
3.81 ft-lb/in² <br>@Temperature -22.0 °F |
ISO 180-A |
| 15.0 kJ/m² <br>@Temperature 23.0 °C |
7.14 ft-lb/in² <br>@Temperature 73.4 °F |
ISO 180-A | |
| Izod Impact, Unnotched (ISO) | NB <br>@Temperature 23.0 °C |
NB <br>@Temperature 73.4 °F |
ISO 180-U |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear, Parallel to Flow | 76.0 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
42.2 µin/in-°F <br>@Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
| CTE, linear, Transverse to Flow | 80.0 µm/m-°C <br>@Temperature 23.0 - 55.0 °C |
44.4 µin/in-°F <br>@Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
| Deflection Temperature at 0.46 MPa (66 psi) | 95.0 °C | 203 °F | ISO 75-1,-2 |
| Deflection Temperature at 1.8 MPa (264 psi) | 85.0 °C | 185 °F | ISO 75-1,-2 |
| Vicat Softening Point | 103 °C <br>@Load 5.10 kg |
217 °F <br>@Load 11.2 lb |
120°C/h; ISO 306 |
| Flammability, UL94 | V-0 <br>@Thickness 1.50 mm |
V-0 <br>@Thickness 0.0591 in |
|
| 5VB <br>@Thickness 2.00 mm |
5VB <br>@Thickness 0.0787 in |
||
| 5VA <br>@Thickness 3.00 mm |
5VA <br>@Thickness 0.118 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm | 1.00e+16 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+16 ohm | 1.00e+16 ohm | IEC 60093 |
| Dielectric Constant | 3.1 <br>@Frequency 1.00e+6 Hz |
3.1 <br>@Frequency 1.00e+6 Hz |
IEC 60250 |
| 3.2 <br>@Frequency 100 Hz |
3.2 <br>@Frequency 100 Hz |
IEC 60250 | |
| Dielectric Strength | 30.0 kV/mm <br>@Thickness 1.00 mm |
762 kV/in <br>@Thickness 0.0394 in |
IEC 60243-1 |
| Dissipation Factor | 0.0050 <br>@Frequency 100 Hz |
0.0050 <br>@Frequency 100 Hz |
IEC 60250 |
| 0.0070 <br>@Frequency 1.00e+6 Hz |
0.0070 <br>@Frequency 1.00e+6 Hz |
IEC 60250 | |
| Comparative Tracking Index | 300 V | 300 V | Solution A; IEC 60112 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Temperature | 240 °C | 464 °F | Injection molding; ISO 294 |
| Mold Temperature | 80.0 °C | 176 °F | Injection molding; ISO 294 |
| Injection Velocity | 240 mm/sec | 9.45 in/sec | ISO 294 |