Conforma Clad WC 200 Tungsten Carbide-Nickel Cladding

Category Ceramic , Carbide , Metal , Metal Matrix Composite , Nonferrous Metal , Nickel Alloy , Other Engineering Material , Ceramic/Metallic Coating
Manufacturer Conforma Clad, a Kennemetal Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Conforma Clad WC 200 Tungsten Carbide-Nickel Cladding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conforma Clad is a targeted wear solution applied to vulnerable surfaces of a component. The wear protection is delivered via a proprietary cloth or slurry, ranging from 0.020" to 0.120" thick.If applied by the cloth system: The cloth is heavily loaded with WC particles held together by a binder. The cloth is adhered to the substrate and is overlayered with a brazing cloth of filler material. The component is then placed in a vacuum furnace where the brazing material melts and infiltrates the WC cloth.If applied by the slurry system: The component is also vacuum brazed. It is well suited for complex shapes.The result from either delivery system is a surface that is metallurgically bonded to the substrate, extremely durable, and is highly resistant to erosion, abrasion, and corrosion. Uses include coatings for plastics processing equipment.Information provided by Conforma Clad, a Kennametal Company.Composition Notes: WC includes cobalt-bonded WC. Total carbide loading from other carbide formation is 68%.
Physical Properties Metric English Comments
Density 12.2 g/cc
0.440 lb/in³
Porosity <= 3.0 %
<= 3.0 %
Mechanical Properties Metric English Comments
Hardness, Rockwell C 64 - 70
64 - 70
Average for the composite. WC particles are about 2000 Vickers DPH<sub>50g</sub> surrounded by a two phase matrix of 300-800 Vickers DPH<sub>50g</sub> (30-64 HRC).
Adhesive Bond Strength >= 483 MPa
>= 70000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 33.1 W/m-K
230 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Chromium, Cr 6.0 %
6.0 %
Nickel, Ni 30 %
30 %
Other 2.0 %
2.0 %
WC 62 %
62 %