Zig Sheng Industrial ZISAMIDE® HP2201 Nylon 6

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Zig Sheng Industrial Co
Trade Name ZISAMIDE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zig Sheng Industrial ZISAMIDE® HP2201 Nylon 6.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ZISAMIDE® HP2201 is a spinning grade Polyamide 6. Application: textile fulldullInformation provided by ZIG SHEN Industrial Co., LTD.
Physical Properties Metric English Comments
Melt Index of Compound 190 - 240 g/10 min
190 - 240 g/10 min
Thermal Properties Metric English Comments
Melting Point 220 - 225 °C
428 - 437 °F
Component Elements Properties Metric English Comments
TiO2 1.5 - 1.7 %
1.5 - 1.7 %
Processing Properties Metric English Comments
Moisture Content <= 0.060 %
<= 0.060 %
Descriptive Properties Value Comments
Amino End Group (meq/kg) 44 ± 3
Extractable (%max) < 0.6