Material Notes:
Blend of H4543 and self-made flame retardant material. Flame retardant, good balance of low and high temperature properties. Applications requiring flame retardancy, such as wires, cables and optical fiber.Information provided by Chengdu Polyster Co., Ltd.
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
ISO 1183
Melt Flow 5.0 - 10 g/10 min
5.0 - 10 g/10 min
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ISO 868
Tensile Strength, Ultimate 22.0 MPa
3190 psi
ISO 527-1
Elongation at Break 350 %
350 %
ISO 527-1
Flexural Modulus 0.0950 GPa
13.8 ksi
ISO 178
Tear Strength 70.0 kN/m
399 pli
ISO 34
Thermal Properties Metric English Comments
Melting Point 194 °C
381 °F
ISO 3146
Brittleness Temperature -60.0 °C
-76.0 °F
ISO 974