Cheng Yu Plastic ML3425 PC, 25% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 30% Glass Filled
Manufacturer Cheng Yu Plastic Company Limited (formerly Luen Cheong Hong)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cheng Yu Plastic ML3425 PC, 25% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.012 cm/cm
0.0060 - 0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 93
93
ASTM D785
Tensile Strength, Yield 108 MPa
15600 psi
ASTM D638
Flexural Yield Strength 172 MPa
24900 psi
ASTM D790
Izod Impact, Notched 1.13 J/cm
2.11 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 149 °C
300 °F
ASTM D648
Flammability, UL94 V-2
V-2