ChevronTexaco Delo® 400 SAE 20

Category Fluid , Lubricant
Manufacturer ChevronTexaco Corp
Trade Name Delo®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ChevronTexaco Delo® 400 SAE 20.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Chevron Delo 400 heavy duty motor oils are exceptional, super premium quality “universal” engine oils which exceed industry and engine manufacturers’ performance requirements.They are formulated utilizing the most advanced additive technology available to provide outstanding engine protection under both pre- and post-1998 EPA standards for exhaust particulate emissions for on highway diesel trucks, using both high and low sulfur diesel fuels.Chevron Delo 400 SAE 10W, 20, 30, 40 and 50 are manufactured using carefully selected premium paraffinic base oils and an optimal blend of the latest technology in dispersant, detergent, oxidation inhibition, anti-wear, corrosion inhibition, and defoaming additives.Chevron Delo 400 SAE 10W-30 is formulated with ISO-SYN™ base stocks.Appliactions: Chevron Delo 400 oils are mixed-fleet motor oils recommended for all four-stroke gasoline diesel engines operating under severe service and subjected to wide variations in climactic conditions.Chevron Delo 400 oils are excellent for use in new advanced engines developed in response to 1998 lower exhaust particulate emissions with features such as four-valve heads, turbo charging, retarded fuel injections timing, direct injection, shorter piston crowns, higher power density, peak firing pressures up and beyond 2300 psi, intercooling, full electronic management of fuel systems, and exhaust particulate traps.Chevron Delo 400 oils are also formulated for superior performance in older engines using both normal, high and low sulfur diesel fuels.Chevron Delo 400 oils are not recommended for use in DDC two-stroke engines.Chevron Delo 400 SAE 30 can be used in in powershift transmissions requiring Caterpillar TO 2 or an Allison C4 fluid.Chevron Delo 400 SAE 10W, 20, 30, and 40 are authorized by USDA for use in federally inspected meat and poultry plants as H2 lubricants with no food contact.
Physical Properties Metric English Comments
API Gravity 30.7 °
30.7 °
Viscosity Measurement 104
104
Viscosity Index; ASTM D2270
Kinematic Viscosity at 40°C (104°F) 68 cSt
68 cSt
ASTM D445
Kinematic Viscosity at 100°C (212°F) 8.9 cSt
8.9 cSt
ASTM D445
Ash 1.18 %
1.18 %
Sulfated Ash wt%
Thermal Properties Metric English Comments
Pour Point -30.0 °C
-22.0 °F
ASTM D97
Flash Point 238 °C
460 °F
ASTM D92
Component Elements Properties Metric English Comments
Phosphorous, P 0.114 %
0.114 %
Zinc, Zn 0.127 %
0.127 %
Chemical Properties Metric English Comments
Total Base Number 9.2
9.2
ASTM D2896