Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CeramTec Rubalit® A 1898 Alumina, 98%

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer CeramTec North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CeramTec Rubalit® A 1898 Alumina, 98%.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Rubalit® A 1898 (98%) was specifically developed in response to electrical and electronic engineering needs. In conjunction with CeramTec's complementary metallization systems, a vacuum-tight bond of high strength is achieved. Rubalit® A 1898 has high dielectric strength and volume resistivity combined with good thermal conductivity. The metallization system consists of tungsten overplated with nickel for effective hard solder wetting properties. For soft soldering purposes, an additional tin layer can be applied. The use of special brazing materials (e.g., AgCu solder) assures a reliable interface during processing and handling. Brazing is performed in an inert gas atmosphere or vacuum, using temperature/time profiles specifically adapted for each product. The result is a vacuum-tight ceramic-to-metal joint with high bond strength. Glazes can be optionally applied to each product in order to prevent contamination of the ceramic surface, which helps preserve the ceramic's insulating properties under operating conditions.
Physical Properties Metric English Comments
Density 3.80 g/cc
0.137 lb/in³
Water Absorption 0.00 %
0.00 %
Permeability 0.00
0.00
%, Gas
Weibull Modulus 11
11
Mechanical Properties Metric English Comments
Vickers Microhardness 1400
1400
HV 10
Modulus of Elasticity 350 GPa
50800 ksi
Flexural Strength 400 MPa
58000 psi
Compressive Strength 3800 MPa
551000 psi
Poissons Ratio 0.22
0.22
Fracture Toughness 4.10 MPa-m½
3.73 ksi-in½
K<sub>IC</sub>
Shear Modulus 143 GPa
20700 ksi
Calculated
Thermal Properties Metric English Comments
CTE, linear 5.40 µm/m-°C

@Temperature 20.0 - 200 °C
3.00 µin/in-°F

@Temperature 68.0 - 392 °F
6.90 µm/m-°C

@Temperature 20.0 - 400 °C
3.83 µin/in-°F

@Temperature 68.0 - 752 °F
7.70 µm/m-°C

@Temperature 20.0 - 600 °C
4.28 µin/in-°F

@Temperature 68.0 - 1110 °F
8.50 µm/m-°C

@Temperature 20.0 - 1000 °C
4.72 µin/in-°F

@Temperature 68.0 - 1830 °F
Specific Heat Capacity 0.900 J/g-°C

@Temperature 20.0 - 100 °C
0.215 BTU/lb-°F

@Temperature 68.0 - 212 °F
Average
Thermal Conductivity 26.0 W/m-K

@Temperature 20.0 - 100 °C
180 BTU-in/hr-ft²-°F

@Temperature 68.0 - 212 °F
Component Elements Properties Metric English Comments
Al2O3 98 %
98 %
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+7 ohm-cm

@Temperature 800 °C
>= 1.00e+7 ohm-cm

@Temperature 1470 °F
>= 1.00e+11 ohm-cm

@Temperature 400 °C
>= 1.00e+11 ohm-cm

@Temperature 752 °F
>= 1.00e+14 ohm-cm

@Temperature 20.0 °C
>= 1.00e+14 ohm-cm

@Temperature 68.0 °F
Dielectric Constant 10

@Frequency 1.00e+7 Hz
10

@Frequency 1.00e+7 Hz
Dielectric Strength 25.0 kV/mm
635 kV/in
Dissipation Factor 0.0010

@Frequency 1.00e+7 Hz
0.0010

@Frequency 1.00e+7 Hz
Users viewing this material also viewed the following: