Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Carlson C 800 Nickel-Iron-Chromium Alloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Carlson
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Carlson C 800 Nickel-Iron-Chromium Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionCarlson Alloy C 800 is a nickel-iron-chromium alloy, combining high strength with excellent resistance to oxidation and carburization at elevated temperatures. This alloy resists sulfur attack, internal oxidation, scaling and corrosion in a wide variety of industrial atmospheres.The high chromium content of C 800 assures good resistance to oxidation, while the nickel content imparts a fair degree of resistance to stress corrosion cracking.Carlson Alloy C 800H is essentially the same alloy as C 800 except the carbon content is restricted to the upper portion of the specified range. C 800H also receives a solution-anneal which produces a coarser grain structure. This assures higher creep and rupture strengths, enabling C 800H to be used in applications that require prolonged exposure at elevated temperatures and/or in corrosive environments.ApplicationsChemical Processing – heat exchangers for nitric acid production; calciners, dryers and recuperators in soda ash plants; process equipment in fiberglass and ore processing plants.Petroleum and Petrochemical – tubing for hydrotreaters and effluent coolers; tubing, manifolds, pigtails and quench lines in hydrogen reformers; flare tips for incinerating waste gasses in refineries; reformer tubing, catalyst grid supports and converters for ammonia production; ethylene furnaces; tubing, bends and flanges for vinyl chloride production; steam superheaters for styrene production.Power Generation – boiler superheaters and reheater tubes and shields; gas turbine combustion cans, transition liners and diffusers.Thermal Processing – baskets and boxes, fixtures and radiant tubes for heat treat furnaces.Steel Production – coke plat quench-car liners and process piping; steam methane reformers and recuperators for direct reduction of iron ore.Information provided by Carlson
Physical Properties Metric English Comments
Density 7.94 g/cc
0.287 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 517 MPa
>= 75000 psi
Tensile Strength, Yield >= 207 MPa

@Strain 0.200 %
>= 30000 psi

@Strain 0.200 %
Elongation at Break >= 30 %
>= 30 %
Modulus of Elasticity 197 GPa
28500 ksi
132 GPa

@Temperature 871 °C
19200 ksi

@Temperature 1600 °F
169.9 GPa

@Temperature 427 °C
24640 ksi

@Temperature 800 °F
Thermal Properties Metric English Comments
CTE, linear 18.4 µm/m-°C

@Temperature 21.1 - 871 °C
10.2 µin/in-°F

@Temperature 70.0 - 1600 °F
Melting Point 1357 - 1385 °C
2475 - 2525 °F
Solidus 1357 °C
2475 °F
Liquidus 1385 °C
2525 °F
Component Elements Properties Metric English Comments
Aluminum, Al 0.15 - 0.60 %
0.15 - 0.60 %
Carbon, C <= 0.010 %
<= 0.010 %
Chromium, Cr 19 - 23 %
19 - 23 %
Copper, Cu <= 0.75 %
<= 0.75 %
Iron, Fe >= 39.5 %
>= 39.5 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Nickel, Ni 30 - 35 %
30 - 35 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.015 %
<= 0.015 %
Titanium, Ti 0.15 - 0.60 %
0.15 - 0.60 %
Electrical Properties Metric English Comments
Magnetic Permeability 1.014
1.014
200 Oersted
Curie Temperature -115 °C
-175 °F