Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Saint-Gobain Perfomance Plastics
Trade Name Meldin®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin® 5330 BearingSpecify Meldin 5330 when part requirements include structural integrity and high resistance to thermal expansion. This material exhibits good wear properties and dimensional stability, making it an excellent candidate for bearing applications.Applications include:Compressor Valve Plates and Valve Rings, Transmission Thrust Washers and Rings, and Vanes for Air Motors and PumpsInformation provided by Saint Gobain Performance Products.
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Water Absorption 0.60 %
0.60 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 107
107
ASTM D785
Tensile Strength 220.5 MPa
31980 psi
ASTM D638
Elongation at Yield 1.5 %
1.5 %
ASTM D638
Flexural Strength 354 MPa
51300 psi
ASTM D790
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Compressive Strength 238 MPa
34500 psi
ASTM D695
Thermal Properties Metric English Comments
CTE, linear 144 µm/m-°C

@Temperature 24.0 - 149 °C
80.0 µin/in-°F

@Temperature 75.2 - 300 °F
ASTM E831-93
Thermal Conductivity 0.910 W/m-K
6.32 BTU-in/hr-ft²-°F
ASTM F433
Deflection Temperature at 1.8 MPa (264 psi) 316 °C
601 °F
ASTM D648