CPC - Vycom POLYCARVE™ Coextruded High Density Sheet (HDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer CPC - Vycom Co.
Trade Name POLYCARVE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CPC - Vycom POLYCARVE™ Coextruded High Density Sheet (HDPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyCarve™ thermoplastic engraving sign stock made to permanently resist the destructive outdoor elements, and certain indoor environments. PolyCarve is a high density, UV stabilized polyethylene consisting of two skins (nominal thickness of .090-.100") outside a core of a different color. This creative color contrast makes it ideal for engraving signs, pictures, company logos and more.FEATURES AND BENEFITS UV Stable- Polycarve is stabilized for long outdoor exposure. Colors- Polycarve is available in many standard color sequences. Strength- Polycarve has excellent physical properties to endure the test of time. Machinability- Polycarve is easily machined and finished with conventional tooling. Consistency- Polycarve is extruded for the best dimensional tolerances and consistency.Information provided by Compression Polymers Corp - Vycom
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 5.0 hour
>= 5.0 hour
F50; ASTM D1693
>= 500 hour
>= 500 hour
F50; ASTM D2561
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 30.3 MPa
4400 psi
ASTM D638
Elongation at Break >= 600 %
>= 600 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Tensile Impact 53.4 J/cm
100 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C
172 °F
ASTM D648
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Brittleness Temperature <= -7.78 °C
<= 18.0 °F
ASTM D746