Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CMW® ELKONIUM 301 platinum based alloy

Category Metal , Nonferrous Metal , Precious Metal , Platinum Alloy
Manufacturer CMW Inc.
Trade Name ELKONIUM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CMW® ELKONIUM 301 platinum based alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Platinum has complete freedom from atmospheric corrosion and is preferred for devices that have low closed forces and where surety of making a circuit may be a problem. It has a high melting point (1769(C) and good resistance to forming arcs. Low electrical conductivity (15% IACS) limits its application to low currents, usually below 5 amperes. Because of the high cost of the platinum ELKONIUM alloys, they are almost always supplied as composite contacts with thin facings of the ELKONIUM metal (silver brazed to nickel plated steel backings in the form of rivets, screws and weld buttons).ELKONIUM® 32 and ELKONIUM® 301 alloys are made up of platinum-iridium materials. Iridium hardens platinum without affecting its tarnish resistance. ELKONIUM 32 alloy contains sufficient iridium to harden the metal to the degree that it resists mechanical deformation and wear in applications that have high closed forces and high impact. Aircraft magnetos and telegraph keys are typical applications, which use the hardness qualities of this alloy. ELKONIUM 301 alloy contains less iridium and is softer and more ductile. It retains the excellent tarnish resistance of platinum and performs reliably in sensitive instruments and low force devices.Information provided by CMW Inc.
Physical Properties Metric English Comments
Density 21.5 g/cc
0.777 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell 15T 90
90
annealed
95
95
cold worked
Tensile Strength, Ultimate 517 MPa
75000 psi
annealed
827 MPa
120000 psi
cold worked
Elongation at Break 5.0 %
5.0 %
cold worked
12 %
12 %
annealed
Component Elements Properties Metric English Comments
Iridium, Ir 15 %
15 %
Platinum, Pt 85 %
85 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000287 ohm-cm
0.0000287 ohm-cm
6 % IACS
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved