Material Notes:
Alloy especially suited to applications in electronics and electro technology. This doped copper, displays high electrical and thermal conductivity, good mechanical properties and excellent temperature stability. CUPROFOR® is used in the manufacture of high power transistor supports, integrated circuits, electrical contacts and shunts.Applications: ElectronicsHeat sinks for power transistorsCUPROFOR® properties includeThermal conductivity to dissipate heatTemperature resistance permitting Pb/Sn soldering of the chip without loss of mechanical properties Mechanical strength to prevent deformation of heat dissipaters when moulding. CUPROFOR® can play an important part in the manufacture of power transistor heat sinks.For this application, CLAL offer 1/2 hard profile strips (condition TL2) in long length coils which can be delivered :totally or partially Ni coated, with an inlay of Pb/Sn, Ag or other material.Support media for printed circuitsThis application uses the following properties :temperature resistance, thus permitting the soldering of the integrated circuit of the DIE PAD, without loss of hardness in the support mediaOutstanding mechanical properties which guarantees the mechanical strength of the LEADSA high deformation capacity gives suitability to form external LEADS.For this application, CLAL, upon request offer long length tapes : a high standard of geometrical and dimensional accuracya stress relieving treatment to maintain that the LEADS TIPS are coplanar about the DIE PAD.The electro-technical fieldElectrical contactsContact mountsPushbuttonsConductive partsElectrical connections and terminals.Other fieldsHeat exchangersSeals and washersDephasing rings.Information provided by CLAL-MSX
Physical Properties Metric English Comments
Density 8.90 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Vickers 115 - 140
115 - 140
112

@Temperature 500 °C,
Time 1800 sec
112

@Temperature 932 °F,
Time 0.500 hour
Isotherm
114

@Temperature 500 °C,
Time 600 sec
114

@Temperature 932 °F,
Time 0.167 hour
Isotherm
117

@Temperature 500 °C,
Time 180 sec
117

@Temperature 932 °F,
Time 0.0500 hour
Isotherm
120

@Temperature 350 °C,
Time 180 sec
120

@Temperature 662 °F,
Time 0.0500 hour
Isotherm
120

@Temperature 500 °C,
Time 60.0 sec
120

@Temperature 932 °F,
Time 0.0167 hour
Isotherm
120

@Temperature 350 °C,
Time 600 sec
120

@Temperature 662 °F,
Time 0.167 hour
Isotherm
120.5

@Temperature 350 °C,
Time 60.0 sec
120.5

@Temperature 662 °F,
Time 0.0167 hour
Isotherm
121

@Temperature 350 °C,
Time 30.0 sec
121

@Temperature 662 °F,
Time 0.00833 hour
Isotherm
121

@Temperature 350 °C,
Time 1800 sec
121

@Temperature 662 °F,
Time 0.500 hour
Isotherm
121

@Temperature 500 °C,
Time 30.0 sec
121

@Temperature 932 °F,
Time 0.00833 hour
Isotherm
122

@Temperature 500 °C,
Time 10.0 sec
122

@Temperature 932 °F,
Time 0.00278 hour
Isotherm
122

@Temperature 350 °C,
Time 0.000 sec
122

@Temperature 662 °F,
Time 0.000 hour
Isotherm
122

@Temperature 350 °C,
Time 10.0 sec
122

@Temperature 662 °F,
Time 0.00278 hour
Isotherm
123

@Temperature 500 °C,
Time 0.000 sec
123

@Temperature 932 °F,
Time 0.000 hour
Isotherm
Tensile Strength, Ultimate 350 - 440 MPa
50800 - 63800 psi
Tensile Strength, Yield >= 300 MPa

@Strain 0.200 %
>= 43500 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
L<sub>O</sub>=5.65vS<sub>O</sub>
Modulus of Elasticity 140 GPa
20300 ksi
Thermal Properties Metric English Comments
CTE, linear 16.3 µm/m-°C

@Temperature 0.000 - 500 °C
9.06 µin/in-°F

@Temperature 32.0 - 932 °F
16.4 µm/m-°C

@Temperature 0.000 - 250 °C
9.11 µin/in-°F

@Temperature 32.0 - 482 °F
16.7 µm/m-°C

@Temperature 0.000 - 100 °C
9.28 µin/in-°F

@Temperature 32.0 - 212 °F
Specific Heat Capacity 0.383 J/g-°C
0.0915 BTU/lb-°F
Thermal Conductivity 338 W/m-K
2350 BTU-in/hr-ft²-°F
Melting Point 1080 °C
1980 °F
Component Elements Properties Metric English Comments
Cobalt, Co 0.080 %
0.080 %
Phosphorous, P 0.080 %
0.080 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.00000181 - 0.00000229 ohm-cm
0.00000181 - 0.00000229 ohm-cm