Borealis LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Borealis
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis LE0595-07 Polyethylene Compound, Crosslinkable, Semiconductive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LE0595-07 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. LE0595-07 is a crosslinkable black polyethylene compound, specially designed for bonded semi conductive screen applications. Applications LE0595-07 is intended for semi conductive applications in XLPE medium and high voltage cables. It is developed for constructions with bonded insulation shields. Specifications: AEIC CS7; AEIC CS8; BS 6622; DIN VDE 0276-263; DIN VDE 0276-620; HD 620 S1; HD 632 S1; IEC 60502; IEC 60840; ISO 1872-E/BA, KHXY, 23-G200, C40; ICEA S-93-639; NF C33-223; NF C33-226; UTE C 33-223; and UL 1072.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 1.135 g/cc
0.04100 lb/in³
ASTM D1928C/D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 9.30 MPa
>= 1350 psi
after aging (168h, 150°C)
18.6 MPa
2700 psi
ASTM D638
Elongation at Break 200 %
200 %
25mm/min; ASTM D638
Electrical Properties Metric English Comments
Volume Resistivity <= 100 ohm-cm

@Temperature 90.0 °C
<= 100 ohm-cm

@Temperature 194 °F
ASTM D991
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month