Material Notes:
Borpact™ BC914TF is a high crystalline heterophasic copolymer film resin, based on special Borstar® nucleating technology. This grade is especially developed for the manufacturing of unoriented film for various film processing technologies like cast film process, conventional blown film process with air cooling and roll stack process for thermoformable films/sheets. Optical properties will not be deteriorated as with conventional homo or copolymers at these temperatures. Applications: Borpact™ BC914TF is recommended for label film, lamination films, food packaging, map trays, stand up pouch film, vegetable trays, and inner layer in coextrusion.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ISO 1183
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 1.45 GPa
210 ksi
50% humidity; ISO 178
Charpy Impact, Notched 0.200 J/cm²

@Temperature -20.0 °C
0.952 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
2.50 J/cm²

@Temperature 23.0 °C
11.9 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 166 °C
331 °F
Vicat Softening Point 154 °C

@Load 1.02 kg
309 °F

@Load 2.25 lb
A50; ISO 306