Beijing Ranger Chem E-54 Liquid Epoxy Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Beijing Ranger Chemical Co
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Beijing Ranger Chem E-54 Liquid Epoxy Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by Beijing Ranger Chemical Co.
Physical Properties Metric English Comments
Viscosity 5000 - 10000 cP
5000 - 10000 cP
Descriptive Properties Value Comments
Epoxy Equivalent g/eq 179-192
Feature Solvent Free