Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Bayshore Vinyl Compounds
Trade Name BVC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bayshore Vinyl Compounds BVC 7200-65 Vinyl Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
BVC 7200-65 is an economy grade flexible vinyl formulation designed for easy processing and excellent heat stability. This material will process at high rates with low temperatures and produces a smooth semi-gloss finish. Typical applications are wire coating, weather stripping, tubing, profiles and a variety of injection molded items.Information Provided by Bayshore Vinyl Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 62 - 68

@Time 10.0 sec
62 - 68

@Time 0.00278 hour
ASTM D2240
Tensile Strength at Break 8.89 MPa
1290 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
100% Modulus 0.00393 GPa
0.570 ksi
ASTM D638
Tear Strength 37.7 kN/m
215 pli
ASTM D1004
Thermal Properties Metric English Comments
Brittleness Temperature -36.0 °C
-32.8 °F
Impact Brittleness; ASTM D746
Descriptive Properties Value Comments
Activated Carbon@90°C, % Wt Loss ASTM D1203
Weight Loss (%), ASTM D1239 0.6
Soapy H<sub>2</sub>O Extraction @ 50°C
21
Oil Extraction
34
Hexane Extraction