Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Barlog Plastics KEBAFLEX P D63.1 Polyester-Elastomer, Shore D63

Category Polymer , Thermoplastic , Elastomer, TPE , Polyester TPE , Polyester, TP
Manufacturer Barlog Plastics
Trade Name KEBAFLEX
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Barlog Plastics KEBAFLEX P D63.1 Polyester-Elastomer, Shore D63.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
TPC-ETInformation provided by BARLOG plastics GmbH.
Physical Properties Metric English Comments
Density 1.23 g/cc
0.0444 lb/in³
ISO 1183
Linear Mold Shrinkage, Flow 0.015 cm/cm
0.015 in/in
ISO 294-4
Linear Mold Shrinkage, Transverse 0.015 cm/cm
0.015 in/in
ISO 294-4
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
Tensile Strength at Break 37.0 MPa
5370 psi
ISO 527-1
Elongation at Break >= 500 %
>= 500 %
ISO 527-1
Charpy Impact, Notched NB
NB
ISO 179-1eA
Thermal Properties Metric English Comments
Melting Point 210 °C
410 °F
10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C
185 °F
ISO 75-1/-2
Descriptive Properties Value Comments
Resin Type TPC-ET