Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® PP5026 Polypropylene, Extrusion/Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polypropylene extrusion impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA regulation 21 CFR 177.1520 and is suitable for food contact applications.Applications: Durables, child safety products, corrugated sheet.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D1505
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 102
102
ASTM D-785
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.32 GPa
191 ksi
Secant @ 1% strain; ASTM D-790
Izod Impact, Notched 1.60 J/cm
3.00 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 46.0 °C
115 °F
ASTM D-648
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved