BASF Ultramid® A3ZG7 HP BK 20465 33% Glass Filled PA66 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® A3ZG7 HP BK 20465 33% Glass Filled PA66 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Ultramid A3ZG7 HP BK20465 is a 33% glass reinforced, heat stabilized, impact modified PA66 black with a combination of excellent impact resistance, toughness and strength.Information provided by BASF