| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.96 g/cc | 1.96 g/cc | ASTM D792 |
| Water Absorption | 0.020 % <br>@Temperature 23.0 °C |
0.020 % <br>@Temperature 73.4 °F |
ASTM D570 |
| Linear Mold Shrinkage, Flow | 0.0025 - 0.0080 cm/cm <br>@Thickness 3.20 mm |
0.0025 - 0.0080 in/in <br>@Thickness 0.126 in |
ASTM D955 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 121 | 121 | ASTM D785 |
| Tensile Strength, Yield | 118 MPa | 17100 psi | 5 mm/min; ASTM D638 |
| Elongation at Break | 1.5 % | 1.5 % | 5 mm/min; ASTM D638 |
| Flexural Strength | 186 MPa | 27000 psi | 2.8 mm/min; ASTM D638 |
| Flexural Modulus | 17.7 GPa | 2560 ksi | 2.8 mm/min; ASTM D638 |
| Izod Impact, Notched | 0.588 J/cm <br>@Thickness 3.17 mm |
1.10 ft-lb/in <br>@Thickness 0.125 in |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 1.8 MPa (264 psi) | 270 °C <br>@Thickness 6.40 mm |
518 °F <br>@Thickness 0.252 in |
ASTM D648 |
| Flammability, UL94 | V-0 <br>@Thickness 1.60 mm |
V-0 <br>@Thickness 0.0630 in |
|
| 5VB <br>@Thickness 1.60 mm |
5VB <br>@Thickness 0.0630 in |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+16 ohm-cm <br>@Temperature 23.0 °C |
1.00e+16 ohm-cm <br>@Temperature 73.4 °F |
50% RH; ASTM D257 |
| Dielectric Constant | 5.0 <br>@Frequency 1.00e+6 Hz |
5.0 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |
| Dissipation Factor | 0.0070 <br>@Frequency 1.00e+6 Hz |
0.0070 <br>@Frequency 1.00e+6 Hz |
ASTM D150 |