Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ACC QSil 553 QSI Quantum Silicones Silicone Potting Material

Category Polymer , Thermoset , Silicone
Manufacturer Amber Chemical Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ACC QSil 553 QSI Quantum Silicones Silicone Potting Material.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readily repairable. Key Features: 100% solids - no solvents Long pot life Good elongation Low modulus Material is UL listed.Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Specific Gravity 1.63 g/cc
1.63 g/cc
"B" component
1.63 g/cc
1.63 g/cc
"A" component
Viscosity 6000 cP
6000 cP
"B" component
6000 cP
6000 cP
"A" component
Storage Temperature <= 38.0 °C
<= 100 °F
12 months
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
cured 15 mins @ 150°C
Tensile Strength, Yield 1.72 MPa
249 psi
cured 15 mins @ 150°C
Elongation at Break 240 %
240 %
cured 15 mins @ 150°C
100% Modulus 0.00124 GPa
0.180 ksi
cured 15 mins @ 150°C
Tear Strength 7.89 kN/m
45.0 pli
cured 15 mins @ 150°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.680 W/m-K
4.72 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 240 °C
464 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 4.02e+14 ohm-cm
4.02e+14 ohm-cm
Dielectric Constant 3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
Dissipation Factor 0.0090
0.0090
Comparative Tracking Index 600 V
600 V
Descriptive Properties Value Comments
Color Beige
"A" component
Black
"B" component
Work Life 100 mins
Users viewing this material also viewed the following: