SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP STAT-KON
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP STAT-KON DX92002 PC (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LNP* Stat-kon* DX92002 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive.
Physical Properties Metric English Comments
Density 1.48 g/cc
0.0535 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.0 MPa
9860 psi
5 mm/min; ISO 527
Elongation at Break 2.9 %
2.9 %
5 mm/min; ISO 527
Flexural Strength 111 MPa
16100 psi
2 mm/min; ISO 178
Flexural Modulus 4.60 GPa
667 ksi
2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
4.76 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 20.0 kJ/m²
9.52 ft-lb/in²
80*10*4; ISO 180/1U
Electrical Properties Metric English Comments
Surface Resistance 10000 - 1.00e+7 ohm
10000 - 1.00e+7 ohm
ASTM D257