Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall 1601 Clear 7002 Flexible PVC

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 1601 Clear 7002 Flexible PVC.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flexible polyvinyl chloride compound formulated for USP Class VI applications. The compound possesses exceptional clarity.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.18 - 1.22 g/cc
1.18 - 1.22 g/cc
ASTM D-792
Melt Flow 125 g/10 min

@Load 14.91 kg,
Temperature 175 °C
125 g/10 min

@Load 32.87 lb,
Temperature 347 °F
ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 59 - 65
59 - 65
delayed; ASTM D-2240
Tensile Strength, Yield 14.8 MPa
2150 psi
ASTM D-638
Elongation at Yield 425 %
425 %
ASTM D-638
100% Modulus 0.00517 GPa
0.750 ksi
ASTM D-638
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Melt Temperature 166 °C
330 °F