| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.226 g/cc <br>@Pressure 0.10981 MPa,<br> Temperature 160 °C |
0.04429 lb/in³ <br>@Pressure 15.927 psi,<br> Temperature 320 °F |
|
| 1.239 g/cc <br>@Pressure 0.08457 MPa,<br> Temperature 150 °C |
0.04476 lb/in³ <br>@Pressure 12.27 psi,<br> Temperature 302 °F |
||
| 1.252 g/cc <br>@Pressure 0.06417 MPa,<br> Temperature 140 °C |
0.04523 lb/in³ <br>@Pressure 9.307 psi,<br> Temperature 284 °F |
||
| 1.264 g/cc <br>@Pressure 0.0479 MPa,<br> Temperature 130 °C |
0.04566 lb/in³ <br>@Pressure 6.95 psi,<br> Temperature 266 °F |
||
| 1.277 g/cc <br>@Pressure 0.03513 MPa,<br> Temperature 120 °C |
0.04613 lb/in³ <br>@Pressure 5.095 psi,<br> Temperature 248 °F |
||
| 1.289 g/cc <br>@Pressure 0.02527 MPa,<br> Temperature 110 °C |
0.04657 lb/in³ <br>@Pressure 3.665 psi,<br> Temperature 230 °F |
||
| 1.301 g/cc <br>@Pressure 0.01779 MPa,<br> Temperature 100 °C |
0.04700 lb/in³ <br>@Pressure 2.580 psi,<br> Temperature 212 °F |
||
| 1.312 g/cc <br>@Pressure 0.01223 MPa,<br> Temperature 90.0 °C |
0.04740 lb/in³ <br>@Pressure 1.774 psi,<br> Temperature 194 °F |
||
| 1.324 g/cc <br>@Pressure 0.00820 MPa,<br> Temperature 80.0 °C |
0.04783 lb/in³ <br>@Pressure 1.19 psi,<br> Temperature 176 °F |
||
| 1.335 g/cc <br>@Pressure 0.00534 MPa,<br> Temperature 70.0 °C |
0.04823 lb/in³ <br>@Pressure 0.775 psi,<br> Temperature 158 °F |
||
| 1.346 g/cc <br>@Pressure 0.00337 MPa,<br> Temperature 60.0 °C |
0.04863 lb/in³ <br>@Pressure 0.489 psi,<br> Temperature 140 °F |
||
| 1.357 g/cc <br>@Pressure 0.00205 MPa,<br> Temperature 50.0 °C |
0.04902 lb/in³ <br>@Pressure 0.297 psi,<br> Temperature 122 °F |
||
| 1.367 g/cc <br>@Pressure 0.00120 MPa,<br> Temperature 40.0 °C |
0.04939 lb/in³ <br>@Pressure 0.174 psi,<br> Temperature 104 °F |
||
| 1.378 g/cc <br>@Pressure 0.000670 MPa,<br> Temperature 30.0 °C |
0.04978 lb/in³ <br>@Pressure 0.0972 psi,<br> Temperature 86.0 °F |
||
| 1.388 g/cc <br>@Pressure 0.000360 MPa,<br> Temperature 20.0 °C |
0.05014 lb/in³ <br>@Pressure 0.0522 psi,<br> Temperature 68.0 °F |
||
| 1.398 g/cc <br>@Pressure 0.000180 MPa,<br> Temperature 10.0 °C |
0.05051 lb/in³ <br>@Pressure 0.0261 psi,<br> Temperature 50.0 °F |
||
| 1.408 g/cc <br>@Pressure 0.0000800 MPa,<br> Temperature 0.000 °C |
0.05087 lb/in³ <br>@Pressure 0.0116 psi,<br> Temperature 32.0 °F |
||
| 1.418 g/cc <br>@Pressure 0.0000400 MPa,<br> Temperature -10.0 °C |
0.05123 lb/in³ <br>@Pressure 0.00580 psi,<br> Temperature 14.0 °F |
||
| 1.427 g/cc <br>@Pressure 0.0000100 MPa,<br> Temperature -20.0 °C |
0.05155 lb/in³ <br>@Pressure 0.00145 psi,<br> Temperature -4.00 °F |
||
| Solubility in Water | 0.18 % | 0.18 % | |
| Molecular Weight | 147.44 g/mol | 147.44 g/mol | |
| Vapor Pressure | 0.00100 bar | 0.750 torr |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | -15.0 °C | 5.00 °F | Freezing Point |
| Boiling Point | 156 °C <br>@Pressure 1.013 MPa |
313 °F <br>@Pressure 146.9 psi |
|
| Flash Point | 73.0 °C | 163 °F | TAG closed cup |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Critical Pressure | 40.0 bar | 30000 torr | |
| Critical Temperature | 403 °C | 757 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Moisture Content | <= 0.20 % | <= 0.20 % | ASTM D3401/B, ASTM E1064 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Clear to light yellow liquid, free from visible matter or particles | |
| Color | <200 | APHA, ISO 2211 |
| Composition | <0.1% | Acidity (as HCL) |
| <0.5% | Sum of ethers | |
| <10 mg/kg | Free chlorine, ASTM D4755 | |
| >98% | 1,2,3-Trichloropropane | |
| Flammability limits | 3.2-12.6% |