Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 541-25G Nylon 66, 25% Glass Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 541-25G Nylon 66, 25% Glass Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Nylon 66, 25% glass reinforced for extrusion applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
ASTM D792
Water Absorption 1.0 %
1.0 %
24 hrs; ASTM D570
Moisture Absorption at Equilibrium 1.8 %
1.8 %
50% RH; ASTM D570
Water Absorption at Saturation 6.2 %
6.2 %
ASTM D570
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 171 MPa
24800 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 7.70 GPa
1120 ksi
ASTM D790
Izod Impact, Notched 0.960 J/cm
1.80 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 251 °C
484 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 246 °C
475 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 246 °C
475 °F
ASTM D648