Unifrax Fiberfrax® Fibermax® Caulk

Category Ceramic
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Fibermax® Caulk.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fibermax caulk is a high-temperature blend of Fiberfrax bulk fibers, Fibermax polycrystalline high-alumina fibers, and inorganic binder. This product is available in convenient-to-use caulking tubes. With a temperature grade rating of 1538°C (2800°F), it can be used to caulk joints and cracks in both high-temperature Fiberfrax lining systems and conventional refractories. Fibermax caulk is also used as a patching material around deteriorating burner blocks.Typical ApplicationsCaulk for cracks in refractory and module liningsPatching around burner blocksInformation Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.160 - 0.240 g/cc
0.00579 - 0.00868 lb/in³
Dry
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1427 °C
2601 °F
Recommended Operating Temperature
Shrinkage 1.5 - 2.5 %

@Temperature 1430 °C,
Time 86400 sec
1.5 - 2.5 %

@Temperature 2600 °F,
Time 24.0 hour
Descriptive Properties Value Comments
Appearance Blue gel
Temperature Grade (°F) 2800