Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ashley Polymers Ashlene® 527LDMS Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ashley Polymers Ashlene® 527LDMS Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A very high impact Nylon 66 with Molybdenum disulfide designed to combine high impact with a reduced co-efficient of friction.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
ASTM D570
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 113
113
ASTM D785
Tensile Strength, Ultimate 41.0 MPa
5950 psi
ATSM D638
Elongation at Break 70 %
70 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 9.08 J/cm
17.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 254 °C
489 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 213 °C
415 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 63.0 °C
145 °F
ASTM D648