Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
Nylene® Naxel™ B720 Polycarbonate/PBT Alloy Description: Naxel™ B720 is a Polycarbonate/PBT alloy. Information provided by Custom Resins. ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers PC-1004 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers PC-1006 Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | Test Method A (0.125 in bar); ASTM D256 |
Network Polymers PC-1006 L Description: Colors and Natural Polycarbonate with UVInformation provided by Network Polymers Inc. |
|||
Izod Impact, Notched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Elastoblend® PA6 IM L W Availability: North AmericaForms: PelletsAdditive: Impact Modifier and LubricantFeatures: Impact Modified and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.. |
|||
Izod Impact, Notched | 9.61 J/cm @Thickness 3.17 mm |
18.0 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Techmer ES Plastiblend® TPX-HTN-000CA Availability: North AmericaForms: Pellets Features: High Heat ResistanceInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 200 4 Polycarbonate, General Purpose CALIBRE® 200 series are general purpose, UL listed Polycarbonate resins formulated to comply with the applicable FDA and European regulations governing food contact(1). CALIBRE 200 series resins .. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM Data |
Styron CALIBRE™ 300 4 Polycarbonate, General Purpose CALIBRE® 300 series are general purpose, UL listed polycarbonate resins. CALIBRE 300 series resins exhibit an excellent physical property balance of heat resistance, transparency and impact stren.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256-92 |
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256; Double 15° Notch at 73°F |
Westlake Plastics Lennite® Ultra High Molecular Weight Polyethylene Lennite UHMW-PE is a low friction engineering plastic with excellent chemical resistant and abrasive wear resistance. It is widely used in conveyors, packaging machinery, and food processing machin.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 527 Nylon 66 A very high impact, slightly lubricated, nylon resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256 |
Applied Composites 8072 Polyester SMC Industry Application: TransportationProduct Application: AutomotiveDistinct Features: Zero Shrink, Superior Class A Finish, Improved Impact, Accepts Mold CoatingInformation provided by Applied Compo.. |
|||
Izod Impact, Notched | 9.61 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
18.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall 7020 Rigid PVC, Extrusion Georgia Gulf 7020 is a special purpose rigid PVC profile extrusion compound designed for thin-wall applications requiring the following properties: Impact Strength & ToughnessDimensional StabilityF.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D-256 |
Axiall 7048A Rigid PVC, Extrusion Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D-256 |
Axiall 7181 Rigid PVC, Extrusion Georgia Gulf 7181 is a special purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: WeatherabilityImpact StrengthDimensional StabilityFlame Ret.. |
|||
Izod Impact, Notched | 9.61 J/cm | 18.0 ft-lb/in | ASTM D256-92 |
Lubrizol Stat-Rite® SIS535 Static Control System Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma.. |