Material Notes:
A 43% glass reinforced impact modified Nylon 66.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 103 MPa
14900 psi
ATSM D638
Elongation at Break 3.0 %
3.0 %
ASTM D638
Flexural Modulus 5.50 GPa
798 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 252 °C
486 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 251 °C
484 °F
ASTM D648