Ashley Polymers Ashlene® 257 PPO

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Impact Grade
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 257 PPO.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A high flow grade for applications requiring high impact strength, heat resistance and dimensional stability.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Water Absorption 0.10 %
0.10 %
ASTM D570
Linear Mold Shrinkage 0.0060 cm/cm
0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 50.0 MPa
7250 psi
ATSM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Modulus 2.20 GPa
319 ksi
ASTM D790
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
ASTM D648
Users viewing this material also viewed the following: