| Category | Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber |
| Manufacturer | Arlon |
| Trade Name | |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Arlon CP-375CR Silicone Rubber.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 1.38 g/cc | 1.38 g/cc | Arlon SQA-TMS-024 |
| Outgassing - Total Mass Loss | 0.34 % | 0.34 % | post cured; ASTM E 595 |
| 1.07 % | 1.07 % | cured; ASTM E 595 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 48 | 48 | ASTM D2240 |
| Tensile Strength, Ultimate | 5.86 MPa | 850 psi | ASTM D412 |
| Elongation at Break | 450 % | 450 % | ASTM D412 |
| Tear Strength | 12.3 kN/m | 70.0 pli | Die B; silicone property; ASTM D624 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 232 °C | 450 °F | |
| Minimum Service Temperature, Air | -56.7 °C | -70.0 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 15.0 min @Temperature 177 °C |
0.250 hour @Temperature 350 °F |
|
| 120 min @Temperature 218 °C |
2.00 hour @Temperature 425 °F |
||
| Shelf Life | 6.00 Month @Temperature 23.9 °C |
6.00 Month @Temperature 75.0 °F |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Color | Red | |
| Outgassing - CVCM (%) ASTM E595 | 0.1 | post cured |
| 0.28 | cured |