Material Notes:
Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Side 1; Arlon SQA-TMS-003
102 microns
4.00 mil
Substrate; Arlon SQA-TMS-003
127 microns
5.00 mil
Side 2; Arlon SQA-TMS-003
305 microns
12.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 36
36
Silicone Property; ASTM D2240
Tensile Strength 6.21 MPa
900 psi
Silicone Property; ASTM D412
Elongation at Break 550 %
550 %
Silicone Property; ASTM D412
Tear Strength 14.0 kN/m
80.0 pli
Silicone Property; ASTM D624
Peel Strength 2.56 kN/m
14.6 pli
Bond Strength (S1 to S2); Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability Test 1.1
1.1
Inches; Char Length; FAR 25.853 App F, Pt. 1, S. A1ii
6.3
6.3
Seconds; Flame and Glow Time; FAR 25.853 App F, Pt. 1, S. A1ii
Electrical Properties Metric English Comments
Dielectric Strength 33.3 kV/mm
845 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 10.7
Arlon SQA-TMS-025