Material Notes:
Designation ISO 1874-PA11,M,18-020,GB30Rigid grade with glass beads (30%) filler for injection molding. Available colors: black and natural. Additive free.Outstanding isotropic properties. High compressive strength. Low and homogeneous shrinkage: include 0,5% on average for the design of the mold. High dimensional stability (low moisture absorption).Water potable contact approval WRC 950 1509. UL classification: UL94 HB RTI(C) 65/65/65Example applications: Mechanical parts with high dimensional precision.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Water Absorption 1.3 %
1.3 %
Melt Flow 7.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
7.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.0 MPa
6090 psi
50 mm/min
Elongation at Break 37 %
37 %
Nominal Strain; 50 mm/min
Elongation at Yield 4.0 %
4.0 %
50 mm/min
Tensile Modulus 2.10 GPa
305 ksi
1 mm/min
Charpy Impact Unnotched 5.16 J/cm²
24.6 ft-lb/in²
5.81 J/cm²

@Temperature -30.0 °C
27.7 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.500 J/cm²
2.38 ft-lb/in²
0.470 J/cm²

@Temperature -30.0 °C
2.24 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Flammability, UL94 HB

@Thickness 1.60 mm
HB

@Thickness 0.0630 in
HB

@Thickness 3.10 mm
HB

@Thickness 0.122 in