Lubriplate SYNCOOL 32 Polyglycolester-Based Synthetic Air Compressor Fluid

Category Fluid , Lubricant , Polyglycol
Manufacturer Lubriplate Lubricants
Trade Name SYNCOOL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubriplate SYNCOOL 32 Polyglycolester-Based Synthetic Air Compressor Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
These polyglycolester-based synthetic fluids are designed for rotary screw air compressors. They offer excellent heat transfer properties, low evaporation, high flash points, and outstanding oxidation resistance, eliminating varnish and sludge. Fluid change intervals are 8,000 hours under normal operating conditions. Syncool Series Fluids are available in Pails & Drums.Information provided by Lubriplate
Physical Properties Metric English Comments
Viscosity Measurement 32
32
ISO Grade
156
156
Viscosity Index
Saybolt Viscosity at 100°F 165 SUS
165 SUS
Saybolt Viscosity at 210°F 34 SUS
34 SUS
Kinematic Viscosity at 40°C (104°F) 30 cSt
30 cSt
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Thermal Properties Metric English Comments
Pour Point -51.1 °C
-60.0 °F
Flammability Test 550
550
[°F] Fire Point
Flash Point 252 °C
485 °F
Descriptive Properties Value Comments
SAE No. 10